This is very tricky welding you can use ER NiCr-3 and ENiCrFe-3 consumables. again it depends on which P45 material you are using. but during welding make sure that dilution of SS side base metal is minimum to avoid micro cracks.

Regards,
VJ
On Wed, Nov 30, 2011 at 10:58 AM, Madhu <madhusudan.rout@gmail.com> wrote:
Dear All,

            For    P45 to P8 material welding, which type consumable
can be use,

                    For SMAW/GTAW process.


Thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...