Dear all,

Greetings.

Vessel nozzles are damaged & tilted due to collision with Bridge during transportation to Site. Vessel was fabricated as per ASME SEC VIII DIV 1. Vessel service - Sever Sour service. PWHT is required because of Service requirement.

One nozzle (6" NPS) is tilted and two other nozzles (30 "NPS) are damaged on gasket face and flange face. Shell Material – SA 516 GR 60 HIC NACE (thickness is 19 mm). Please refer attached Photos.

 

I believe Visual Inspection & MT/PT can be performed to detect any surface Crack on the affected Nozzles and Shell surfaces of the Vessel. Ovality shall be checked on the affected Nozzle areas.

Also Visual and MT/PT can be done for ALL WELDS of the Vessels.
 
please advise whther UT is also required.

Please advise the steps to rectify the problem. Also give code reference.

 

Thanks & Regards

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...