Dear hMr. Bagchi

I attached our drawing, do you mean after completion of welding there is no cleaning required?

Regards,
Himan

On Mon, Nov 28, 2011 at 4:11 AM, <snbagchi@aol.in> wrote:
Dear Mr. Himan,

Normally, Inconels are higkly corrosion resistant alloys, which do not need passivation. However, you are advised to show assemby drawing near welded area which needs to be looked into.

S.N.Bagchi.
<snbagchi@aol.in>


-----Original Message-----
From: Himan Nikdin <himannikdin@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sun, Nov 27, 2011 5:15 pm
Subject: [MW:13069] Inconel Passivation


Dear Friends


I have stone trap which will be made from API 5L-X52 that inner side overlaied by Inconel, I want to know we shall clean welded separate pipes welded area by acid pickling or any passivation is mandatory???


I will be appreciated if anybody can help me.


Thank you in advance.
Himan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...