[MW:13039] RE: Dual certification of material (plates/pipes)

Yes it is acceptable. 
 
The verifying documents will be the Material Specifications for the grades which are named and the Material Test Reports (including but not limited to chemistry, mechanical properties and heat treatment condition) for the steel which is supplied.  There is some overlap between different material grades. 
 
Some Customer specifications allow for a 'superior' grade to be substituted without notification for an 'inferior' grade.  For example in pipe; ASTM SA333-6 to be substituted for ASTM SA106-B.  In this example, the SA333-6 is superior and the SA106-B is inferior.  Another case is substitution of forged items for cast items.  Always check your Customer Specifications for restrictions which may supersede Code.  Usually the Owner has requirements regarding substitution and dual-grading.
 
Regards,
 
Darcy Morin
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nadgauda, Subhas
Sent: November 23, 2011 3:45 AM
To: materials-welding@googlegroups.com
Subject: [MW:13035] FW: Dual certification of material (plates/pipes)

 

 

 

Dear all,

 

Is dual certification of pipes / plates acceptable? Please furnish code / amendment reference.

 

Thanks in advance & Regards.

 

Subhas Nadgauda

JACOBS-Navi Mumbai

Mob:09869552260

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...