Re: [MW:13036] joint configuration detail

 Dear Bala,

It is full penetration weld with fillet weld on the other side

With regards

Vimal Kumar
+65 9100 2565

On 23 Nov, 2011, at 8:24 AM, bala krishnan <balakrishnanr1@yahoo.co.in> wrote:

Dear experts ,
  here i attached weld joint detail.
please advise me regard about weld joint configuration.
 
friendly,
bala

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
<123.jpg.bmp>

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...