RE: [MW:13103] what is the root cause for copper crack in saw welding ?

 Hi MPK,
 
 
It's a form of solidification cracking caused  due to localized segregation of low melting elements. Copper is one of the elements which tends to form so, for C.S and high strength and medium strength low alloy steels.
 
Please see the reference below.
 
Thanks.
 
P.Goswami,P.Eng,IWE
 
http://content.lincolnelectric.com/pdfs/knowledge/articles/content/weldcracking.pdf
 

Date: Tue, 29 Nov 2011 16:32:37 +0300
Subject: [MW:13100] what is the root cause for copper crack in saw welding ?
From: ranmi2007@gmail.com
To: materials-welding@googlegroups.com

Dear Experts,
What is the Root cause for copper crack in SAW welding ?

thanks,
MPK


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...