RE: [MW:13023] which is better BW OR BE?

 
 
You are talking about 2 different things.  BE is not the same as BW.  Please let me explain:
 
You should specify BE if you are referring to a specific pipe end or fitting. 
 
BE=bevelled end.  PE=plain end.  TE=threaded end. 
 
If you order an NPS 1 nipple PE/BE, you will receive a nipple that is bevelled one end and the other end is plain. 
 
If drafting an Isometric for example, if you are referring to a joint, then use BW (Butt-weld), SW (Socket-weld), but on the material list, the items will be called out as to their end preparation (BE, PE, TE).
 
Be aware that end preparation differs for Socket-welded joints compared with Butt-welded joints, check your line requirements as per your Engineering department/Customer Specifications. 
 
Warm regards,
 
Darcy Morin


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Alpesh Sakhreliya
Sent: November 18, 2011 2:05 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13016] which is better BW OR BE?

BW end type to be used
 both are same


On Fri, Nov 18, 2011 at 7:32 AM, aslam khan <aslamkhan4u@gmail.com> wrote:
hi friends,
I need your expert opinion,
which is better for fittings e.g Elbows,Tee reducer  END TYPE=BW(butt
weld) or BE(bevel end).i am working on smart software and dealing with
item coding.some people write BE AND some BW as End Type.which is
better to be used ?are these same or different?thanks in advance .

Best Regards
Aslam khan
Descon Engineering Ltd.Pakistan
Cell#+923214217438

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Best Regards,

 

Alpesh Sakhreliya

Technical Services

Gujarat State Petronet Limited

Direct: +91 79 66701527

Mobile:+91 9898265772


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...