Re: [MW:13042] which is better BW OR BE?

Th BW and BE are not same, it is possible to have Butt weld but the ending maybe Beveled End BE or maybe Plained End, PE
 
Normally in piping below 2" welding joints is Socket weld, with PE
 
and above 2" welding joints is Butt Weld with BE, anyhow this may change for each piping class, for confimation please check with your project piping class.
 
Regards,

On Wed, Nov 23, 2011 at 8:30 AM, Dindo <dindodelacruz@gmail.com> wrote:
The difference I would surmise is that PE & BE are BW, PE could be a BW, which is termed as square butt weld. BE would mean that the ends are either singe VEE butt weld, U butt weld, Double Vee Butt weld etc...
 


 
On Wed, Nov 23, 2011 at 2:36 AM, Krishnakumar M S <krishnakumarms01@yahoo.com> wrote:
Dear Aslam,

In piping aspect we use fitting ends shall be " BE " for welded joints and " PE " for plain ends

BW - is used only for the terms in method of fabrication of piping.

pls see the attached doc for further explanation

I hope that you have to understand the two terms.

Regards,

KRISHNAKUMAR.M.S
Piping Engineer
Fact Engineering & Design Organization (FEDO)
KERALA, INDIA


From: aslam khan <aslamkhan4u@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Friday, 18 November 2011 7:32 AM

Subject: [MW:13012] which is better BW OR BE?

hi friends,
I need your expert opinion,
which is better for fittings e.g Elbows,Tee reducer  END TYPE=BW(butt
weld) or BE(bevel end).i am working on smart software and dealing with
item coding.some people write BE AND some BW as End Type.which is
better to be used ?are these same or different?thanks in advance .

Best Regards
Aslam khan
Descon Engineering Ltd.Pakistan
Cell#+923214217438

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...