[MW:13090] RE: 13087] 4130 pipe material

The 4130 is a code of AISI and defines the approximate chemical composition of the steel where in 42 denotes low alloy steel containing approximate 1% Chromium and 0.2% Moly so it is called Chromoly. The 30 mean it contain 0.30% Carbon.

Regards

Vinod Kataria

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vimal Kumar
Sent: Tuesday, November 29, 2011 1:03 PM
To: materials-welding@googlegroups.com
Subject: [MW:13087] 4130 pipe material

 

Dear all, 

            May I know the expert advice on this
1. What is 4130 material
2. 4130 is under which specification
3. If 4130 is a general term for some group of material, what are the material that are called 4130

With regards

Vimal Kumar
+65 9100 2565

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...