[MW:13027] RE: 13026] How is the Recordable UT Output Reg.,

Please elaborate your question a bit further

 

Best Wishes

Aftab Ahmad

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kcrtechnical
Sent: Monday, November 21, 2011 6:04 PM
To: materials-welding@googlegroups.com
Subject: [MW:13026] How is the Recordable UT Output Reg.,

 

Dear Freinds,

 

Can any NDT UT Expert explain me with sample, how is the Out put of Weld Joint Recordable UT

 

Best regards

K C Rayappa

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...