[MW:13014] FW: 13012] RE: 13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

 
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Friday, November 18, 2011 9:25 AM
To: 'sivaselvam@kpoc.com.my'
Subject: RE: 13012] RE: 13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

Please look through Annex-A, if this material falls in to the list mentioned no HIC test is required.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sivaselvam Ponandrum
Sent: Friday, November 18, 2011 1:57 AM
To: materials-welding@googlegroups.com
Subject: [MW:13012] RE: 13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

Hi,

 

Based on the process requirement, the Pipe is specified for NACE Certification, in addition HIC requirement is specified for pipes/ fitting that fabricated from welded plates, also we specified for HIC is not required for seamless pipe / fittings.

 

 

Now for joining two pipes / fittings together whether it is seamless or welded pipe or fittings (fabricated from plates), does the WPS qualification requires HIC Testing?

 

If yes, what is the HIC Testing Procedure & Acceptance Criteria.?

 

 

Case A

 

 

 

 

Case B

 

 

Case C

 

 

Case F

 

 

 

Case G

 

Case I

 

 

 

Regards

 

Siva

 

Asset Integrity

 

Operation Assurance


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Friday, November 18, 2011 12:06 PM
To: materials-welding@googlegroups.com
Cc: Sivaselvam Ponandrum
Subject: [MW:13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

 

Hello,

 

Your query is too general. Can you specify what're the design requirements, wrt PH2S, PCO2, Temperature or any other design variable.

 

What's the material specification for pipes?

 

Appreciate your response.

 

Thanks.

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist & Consultant

Ontario,Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sivaselvam Ponandrum
Sent: Thursday, November 17, 2011 3:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:13008] NACE requirement, does the WPS requirement HIC Test?
Importance: High

 

Dear All,

 

For welding carbon steel pipe with NACE requirement, does the WPS qualification requires HIC Test?

 

 

Regards

 

Siva

 

Asset Integrity

 

Operation Assurance

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...