Friday, November 18, 2011

[MW:13021] Crack in Dishend

Dear All,
 
Attached is the photo of 2:1 Ellipsoidal dish.
 
Material : SA 240 type 201-2.
Chemical Comp : C=0.0995, CR=16.212, Mn=7.345, N=0.727, NI=4.07, P=0.031, S=0.001 & SI=0.465.
Mechanical Property : Yield = 56KSI (min) & UTS = 107KSI.
Condition : Annealed
 
After Forming of dish head(no heat treatment is done) crack is observed.
 
can any one tell the reason of cracking?
 
Regards,
 
Devang Patel

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...