RE: [MW:12581] Tension Test Requirement for SA 283 Gr.C plates

You have to identify heat number and lot number of all these plates, and then decide number of tests.

 

BR

 

HWCai

Sulzer

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pieper QSI
Sent: Thursday, September 29, 2011 12:40 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:12575] Tension Test Requirement for SA 283 Gr.C plates

 

It seems to me that when every plate has similar heat and plate number they will be produced from a coil, especially when the thickness is 6 mm.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens asad azmi
Verzonden: woensdag 28 september 2011 16:29
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12573] Tension Test Requirement for SA 283 Gr.C plates

 

SA 20 is not applicable here.



 

On Wed, Sep 28, 2011 at 2:10 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

One tension test coupon shall be taken from each plate-as-rolled (para 11.1.1 of SA20).

 

Note: plate-as-rolled— the quantity of plate product rolled at one time, either from an individual slab or directly from an ingot.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, September 28, 2011 3:59 PM
To: materials-welding@googlegroups.com
Subject: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates

 

Dear All,

 

Greetings.

 

 

As per MTC for the plates material - SA283GR C,  for a single Heat number( 10K22884)  total 15 Nos of plates are supplied having plate no. 15942 

 

Description of Goods- Hot rolled steel plates with sheared edges. Plates are in Non Heatreated  condition.

 

MTC is showing only  2 tension test results.

 

Please clarify whether only two tension test are acceptable OR there shall be 15 nos of tension test for 15 plates.( 1 tension test for each plate)

 

Thanks & Regards

 

Asad Azmi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

CONFIDENTIALITY NOTICE
The information in this email may be confidential and/or privileged.
This email is intended to be reviewed by only the addressee(s) named
above. If you are not the intended recipient, you are hereby notified
that any review, dissemination, copying, use or storage of this email
and its attachments, if any, or the information contained herein is
prohibited. If you have received this email in error, please
immediately notify the sender by return email and delete this email
from your system. Thank you.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...