Re: [MW:12562] Carbides Precipitates on HAZ ; 625 Overlay on AISI 4130

Dear Sir,
              I think u may have to use a buttering layer.

2011/9/27 K.Babu <kbabupsg@gmail.com>

Gents,

Do you have idea on the Inconel 625 Overlay on the AISI 4130/4140

I used P-GTAW, with 150deg cel as preheat & Max . Inter pass is 240 deg cel, PWHT -590 deg. Cel for 3 hrs to reduce the hardness to below 250 VHN

In micro analysis, HAZ showing the carbide precipitates.

Any idea, on why happened like this?

Regards
 
K.Babu
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...