Dear
Mr.P.Goswami,
Can you explain about PWHT for P.No.8?
What is requirement of Solution Annealing or PWHT for these?

On Mon, Sep 26, 2011 at 8:14 AM, pgoswami <pgoswami@quickclic.net> wrote:
Hi Vijay,
 
As per QW 407.2 a change of PWHT time and temperature is a supplementary essential variable. If there is no requirement of impact properties, the PQR qualified @ 620 deg C of PWHT  may be used as the supporting PQR for performing PWHT @ 670 deg C.
 
Note:- selection of 670 deg C for PWHT would not be right for P1 material due to the fact that it would significantly soften carbon steel.If there is any hardness restriction then the PQR  and the production weld should be done at the same Time and Temperature.
 
Austenitic stainless steels do not require any PWHT ( in the temperature region of 600-700 deg C),except for solution annealing(1000-1040 deg C) to improve mechanical properties and corrosion resistance.
 
Thanks.
 
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vijay Katkar
Sent: Saturday, September 24, 2011 11:06 AM
To: materials-welding@googlegroups.com
Subject: [MW:12516] WPS Heat treatment condition

Dear All,

Regarding heat treatment ,

I have P1 to P8 PQR with following heat treatment,

 

Loading temperature :- 350  ̊C 

 heating rate : 70   ̊C  /hr

Soaking temperature: 620  ̊C

Cooling rate : 70  ̊C/hr

Unloading temperature: 350  ̊C

 

our job requirement is

Loading temperature :- 350  ̊C

heating rate : 70  ̊C/hr

Soaking temperature: 670  ̊C

Cooling rate : 70  ̊C/hr

Unloading temperature: 350  ̊C

 

Is it possible to use above PQR for same job if yes please tell me the reference in section IX. or this not possible then why because above all temperature below lower critical temperature..

please advice your valuable experience..............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
 
 
With Regards
 
 
Srinivasu V
Welding Engineer
ALSTOM Projects India Limited
Durgapur, West Bengal - 713206
Mobile: +91 8016082905
             +91 8768773235

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...