Hello Everyone,

Currently I am qualifying a welding procedure for a pressure equipment
which involves 3.5% Nickel steel. The design code is ASME VIII Div 1,
the query is what is max. permitted HAZ hardness for this material. I
have got two indentations 278 and 280 vickers 10kg in cap HAZ, whilst
the others are well below 250HV10.

WT of the coupon was 10.97mm and I have done a post heating at 350°C
for 2 hours (assuming it would be beneficial to address HIC). I
haven't done any PWHT.

NB: Client is not sure of the permitted max. hardness, from memory -
being a ferritic steel, I would assume max. permitted is 250 for NACE
applications.

I would like a confirmation from the group members, whether my
assumption is correct?

Thanks everyone

Mrithyunjay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...