Re: [MW:12572] RE: 12567] Tension Test Requirement for SA 283 Gr.C plates

thickness of the plate is 6mm.
 
these are seprate rolled plates.
 
Regards

On Wed, Sep 28, 2011 at 2:17 PM, Pieper QSI <pieper-qsi@kpnmail.nl> wrote:

Dear Mr. Azmi,

 

What is the thickness of the plate material, and are these separate rolled plates or manufactured from coil?

In case of production from coil a minimum of 2 tensile specimens need to be tested for each coil, so in this case 2 specimens would be acceptable. See note 1 chapter 3.2 of SA283.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens asad azmi
Verzonden: woensdag 28 september 2011 12:29
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates

 

Dear All,

 

Greetings.

 

 

As per MTC for the plates material - SA283GR C,  for a single Heat number( 10K22884)  total 15 Nos of plates are supplied having plate no. 15942 

 

Description of Goods- Hot rolled steel plates with sheared edges. Plates are in Non Heatreated  condition.

 

MTC is showing only  2 tension test results.

 

Please clarify whether only two tension test are acceptable OR there shall be 15 nos of tension test for 15 plates.( 1 tension test for each plate)

 

Thanks & Regards

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...