Re: [MW:12566] PWHT Requirement for SA 335 P91 (or P no. 5B Group 2)



Dear Asif
Its very critical matril and care shoud be for preheating,postheating and strss relieving.For you,s comfor i am attaching a complete method statement forfabrication of P91 mterial
 
Thanks
 
Mumtaz
 
 
 
 
 
 
On Tue, Sep 27, 2011 at 9:11 AM, ASIF <asifdme@gmail.com> wrote:

Dear experts!


Project : Solar Power Plant
Construction Code ASME B31.1

ASME Sec IX

PWHT Requirement - SA 335 P91 or P no. 5B Group 2 material is not included in 132 Para and Table of B31.1, and also,
ASME Sec IX para QW-407 do not mention this material group.

Client Specification do not mention this requirement separately

Please advise! do we need to go for PWHT ?



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...