SA 20 is not applicable here.


 
On Wed, Sep 28, 2011 at 2:10 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

One tension test coupon shall be taken from each plate-as-rolled (para 11.1.1 of SA20).

 

Note: plate-as-rolled— the quantity of plate product rolled at one time, either from an individual slab or directly from an ingot.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, September 28, 2011 3:59 PM
To: materials-welding@googlegroups.com
Subject: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates

 

Dear All,

 

Greetings.

 

 

As per MTC for the plates material - SA283GR C,  for a single Heat number( 10K22884)  total 15 Nos of plates are supplied having plate no. 15942 

 

Description of Goods- Hot rolled steel plates with sheared edges. Plates are in Non Heatreated  condition.

 

MTC is showing only  2 tension test results.

 

Please clarify whether only two tension test are acceptable OR there shall be 15 nos of tension test for 15 plates.( 1 tension test for each plate)

 

Thanks & Regards

 

Asad Azmi


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...