Monday, September 26, 2011

Re: [MW:12537] spot radiography as per ASME B 31.3



Dear Sir,

Spot Radiography - the spot is selected from the weld length of one joint , the spot may be 300mm lenth minimum as per ASME B 31.3 or API 620 / 650 150 mm length. You may refer the attachment and the details of SPOT Radiography is given there.










Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951


From: "Nachhattar Singh" <nsingh@librainspection.com>
Sent: Mon, 26 Sep 2011 13:36:56
To: <materials-welding@googlegroups.com>
Subject: Re: [MW:12536] spot radiography as per ASME B 31.3

Dear Azhar

 

Your version "Spot Radiography is to be taken on joint but random examination is be selected from the lot"

 

I have the following comments :-

 

01.  In all cases the Radiography is always on the weld joints only

02.  Random is always from the different weld seams of a vessel

 

But the basic question is not yet replied.

 

May be Experts can shed some more light on this matter

 

Best regards

 

 

Nachhattar Singh,

Logo-Libra-Version12

Tel: +91 98201 81158 / +91 22 27580036

Email: nsingh@librainspection.com

            

407/408, Vindhya Commercial Complex,

Sector 11, CBD Belapur

Navi Mumbai - 400 614

Maharashtra, India.

www.librainspection.com

 

PLEASE THINK BEFORE PRINTING

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Azam Mohd
Sent: Monday, September 26, 2011 12:12 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:12533] spot radiography as per ASME B 31.3

 

Dear Azhar,

Spot Radiography is to be taken on joint but random examination is be selected from the lot.

 

Thanks & Regards,

Mohd.Azam

On Mon, Sep 26, 2011 at 8:47 AM, Azhar Ali <aab51214@yahoo.com> wrote:

DEAR EXPERTS

 

let me know the extent of radiography as per ASME B31.3 for normal service.

 

Can any body elaborate the the difference between spot and random examination as per para no.344.1.3. 

 

 

Regards

 

Azhar Ali

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...