Wednesday, September 28, 2011

Re: [MW:12574] Tension Test Requirement for SA 283 Gr.C plates

it is, SA283 cross refers to SA 20

On Wed, Sep 28, 2011 at 7:58 PM, asad azmi <azmiasadayub@gmail.com> wrote:
> SA 20 is not applicable here.
>
>
> On Wed, Sep 28, 2011 at 2:10 PM, Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com> wrote:
>>
>> One tension test coupon shall be taken from each plate-as-rolled (para
>> 11.1.1 of SA20).
>>
>>
>>
>> Note: plate-as-rolled— the quantity of plate product rolled at one time,
>> either from an individual slab or directly from an ingot.
>>
>>
>>
>> From: materials-welding@googlegroups.com
>> [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
>> Sent: Wednesday, September 28, 2011 3:59 PM
>> To: materials-welding@googlegroups.com
>> Subject: [MW:12567] Tension Test Requirement for SA 283 Gr.C plates
>>
>>
>>
>> Dear All,
>>
>>
>>
>> Greetings.
>>
>>
>>
>>
>>
>> As per MTC for the plates material - SA283GR C,  for a single Heat number(
>> 10K22884)  total 15 Nos of plates are supplied having plate no. 15942
>>
>>
>>
>> Description of Goods- Hot rolled steel plates with sheared edges. Plates
>> are in Non Heatreated  condition.
>>
>>
>>
>> MTC is showing only  2 tension test results.
>>
>>
>>
>> Please clarify whether only two tension test are acceptable OR there shall
>> be 15 nos of tension test for 15 plates.( 1 tension test for each plate)
>>
>>
>>
>> Thanks & Regards
>>
>>
>>
>> Asad Azmi
>>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...