Sunday, September 25, 2011

Re: [MW:12524] PQR by E7010 4mm electrode

You are not clear..

Which electride you used for root run ?

What is the job thk ?

What was the root gap ?

I suggest use GTAW root & E 7018 fill.

On 9/25/11, mpk mpk <ranmi2007@gmail.com> wrote:
> Dear Experts,
>
> We have carried out PQR by E7010 4mm electrode for fill passes but it was
> unsuccessful in root bend test.We have carried out same process in repair
> PQR which is successful.
>
> So plz give me your advice which will help me in next PQR.
>
> Thank you...
> MPK
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...