Thursday, September 29, 2011

Re: [MW:12578] 3.5% Nickel steel

Dear Mrithyunjay,
For the 3.5% Nickel steel, it is client to say what hardness they want.
Nace requirement is 248 HV10.
The post heating of 350 Deg.C does not seem to have much impact on HIC testing.
Thanks and Best regards,
K.Rajagopal

On Thu, Sep 29, 2011 at 9:09 AM, mrithyun jay <mrithyun.j@gmail.com> wrote:
Hello Everyone,

Currently I am qualifying a welding procedure for a pressure equipment
which involves 3.5% Nickel steel. The design code is ASME VIII Div 1,
the query is what is max. permitted HAZ hardness for this material. I
have got two indentations 278 and 280 vickers 10kg in cap HAZ, whilst
the others are well below 250HV10.

WT of the coupon was 10.97mm and I have done a post heating at 350°C
for 2 hours (assuming it would be beneficial to address HIC). I
haven't done any PWHT.

NB: Client is not sure of the permitted max. hardness, from memory -
being a ferritic steel, I would assume max. permitted is 250 for NACE
applications.

I would like a confirmation from the group members, whether my
assumption is correct?

Thanks everyone

Mrithyunjay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...