Dear Sir,

You may check your existing PQR soaking temperature tolerance. Normally we will give +/- 40 to 50 degree Celsius. If it is with in that range you may use the same one.



Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951


From: Vijay Katkar <katkar.vijay22@gmail.com>
Sent: Sun, 25 Sep 2011 12:54:36
To: materials-welding@googlegroups.com
Subject: [MW:12516] WPS Heat treatment condition

Dear All,

Regarding heat treatment ,

I have P1 to P8 PQR with following heat treatment,

 

Loading temperature :- 350  ̊C

heating rate : 70   ̊C  /hr

Socking temperature: 620  ̊C

Cooling rate : 70  ̊C/hr

Unloading temperature: 350  ̊C

 

our job requirement is

Loading temperature :- 350  ̊C

heating rate : 70  ̊C/hr

Socking temperature: 670  ̊C

Cooling rate : 70  ̊C/hr

Unloading temperature: 350  ̊C

 

Is it possible to use above PQR for same job if yes please tell me the reference in section IX. or this not possible then why because above all temperature below lower critical temperature..

please advice your valuable experience..............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...