For welding Galvanised items there is no separate filler wire. Before
welding galvanised items, first remove the coating by any remover or
just grind and remove then weld. filler material shall be as per base
metal group and if it is normal carbon steel go with ER 70S2 / E 6013
and so on.....




On Thu, 25 Aug 2011 16:25:38 +0530 wrote
>can any body clarify

which filler wire is required for welding galvanized pipe ?



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...