Dear team members,
Good morning to all, During our on-stream inspection at jetty facilities area, we noticed most of the area in between pipe to pipe support were corroded(crevice corrosion) with sign of metal loss. Some of these piping especially small bore had been lifted, descaled by using hand tool and measured the actual thickness by using pit gauge. But the problem is, how about the big bore piping. Is it any NDT method that we can employ to measure the actual thickness of corroded area without lifting the particular piping. Appreciate if team members can also give the best preventive action. Looking forward for the response. Thank you
Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment