RE: [MW:12230] Gas purging for 12Cr1MoVG

Dear Endri,

 

Taken from API 582

7.3  Back purging is required for the GTAW and GMAW

processes for welding materials having a nominal chromium

content greater than 2 1/4% unless the joint is ground or back

gouged to sound metal.

 

I am agree with sri lakshmi. The main reason using Back Purge is prevents oxidation. But in Golden Joint case you can’t do back purge.

If your PQR accept with no Back Purge, and your Welder is high skill than go a head… But if your PQR stated a back Purge and your skill welder is intermediate,

It’s recommended use back purge.

 

Regards,

Firman Bhaktiwinaya

 

 

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula
Sent: Tuesday, August 16, 2011 10:59 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:12227] Gas purging for 12Cr1MoVG

 

refer para 7.3 of API RP 582

 

On Sun, Aug 14, 2011 at 7:20 PM, Endri Prasetyo

<endri.prasetyo@gmail.com> wrote:

> Dear Mr. Raghuram,

> Can you please share here in which statement of API 582 that mentions about

> it?

> Thanks and regards,

> Endri

> 

> On Sun, Aug 14, 2011 at 2:55 PM, Raghuram Bathula

> <raghurambathula@gmail.com> wrote:

>> 

>> i guess the %Cr <2.25 in this material, in that case back purging is

>> not required as long you have a qualified PQR without purging.

>> Generally purging is recommended for materials with Cr >2.25% (refer

>> API 582).

 

--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...