The best way to measure the corrosion under pipe support is using
LRUT(chime/pipe inspector. But this is a qualitative method and you will
get only the defect grading based on % of wall thickness loss.

regards,

On Thu, 18 Aug 2011 09:15:07 +0800, tong tong wrote:
> Dear team members,
>
> Good morning to all, During our on-stream inspection at jetty
> facilities area, we noticed most of the area in between pipe to pipe
> support were corroded(crevice corrosion) with sign of metal loss.
> Some
> of these piping especially small bore had been lifted, descaled by
> using hand tool and measured the actual thickness by using pit gauge.
> But the problem is, how about the big bore piping. Is it any NDT
> method that we can employ to measure the actual thickness of corroded
> area without lifting the particular piping. Appreciate if team
> members
> can also give the best preventive action. Looking forward for the
> response. Thank you
>
> Regards
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/ [1]
> The views expressed/exchnaged in this group are members personel
> views and meant for educational purposes only, Users must take their
> own decisions w.r.t. applicable code/standard/contract documents.
>
>
> Links:
> ------
> [1] http://materials-welding.blogspot.com/

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...