Re: [MW:12262] welding cupronickel to brass

Dear Sir

U can use ER CuNi(70-30) or ER NiCu7(70-30).
Regards
Sonu Wadhwa (09811067079)
Deals in all types of special welding consumables.



On Thu, Aug 18, 2011 at 9:34 AM, vikas shelke <vikas.shelke84@gmail.com> wrote:
Dear Mr. Kumar,

        ERNiCu-7 SFA 5.14 may be suitable for this.

--  Regards,
 
   Vikas 
 


On Wed, Aug 17, 2011 at 6:17 PM, Kumar <suresh18381@gmail.com> wrote:
Dear all

I would like to know the suitable GTAW filler wire to weld 70/30
Cupronickel material (UNS C71500) to NavalBrass ( UNS C46400).
Expecting anyone of yours kind suggestion.....


thanks and regards

Kumar
Welding Engineer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...