RE: [MW:12278] FW: 11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.

Here is the chart from API which deals with SS mismatches. 
Darcy Morin
 
 
 



-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ahmed osman
Sent: Friday, August 19, 2011 2:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:12273] FW: 11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.

U can use E2209 or E309MoL
Ahmed Osman
Sr Q.C. Eng.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of CHINTUKUMAR GANDHI
Sent: Saturday, May 21, 2011 12:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:11108] DUPLEX S.S. (S.S. 2205) TO AUSTENITIC S.S. (Grade 316L) welding.

Dear Experts,

I come across with very strange welding combination. That is Duplex stainless steel to ausatenitic steel welding. Here Flange is SS 316 L & pipe is duplex stainless steel (2205).

plz guide me abt which filler wire I should use?  & which good engineering practises should adopt during welding.

Chintu Gandhi

Welding Engineer 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...