Thursday, August 18, 2011

Re: [MW:12263] Prequalified WPS


Dear Mr.Arvinda..
 
1.Strictly speaking procedure qualificaiton as per ASME SEC IX- will not validate the qualificaiton as per AWS D.1.1
2. You have to keep the parameters as per the various tables in the sec 3 of AWS D.1.1
 
br,
msms

 
On Wed, Aug 17, 2011 at 1:04 PM, arvinda shan <arvindashan@gmail.com> wrote:
Dear Experts,
 
Plz clarify.
 
  1. PQR is qualified as per sec IX. Can we make WPS for structural as per AWSD1.1 ?
  2. By preparing WPS with pre-qualified procedures as per AWS D1.1 sec.3, how can we prepare? My doubt is as per AWS D1.1 sec 4 WPS, positions are essential.Can we make WPS for all positions in single WPS? How can we make & use pre-qualified procedure.
Arvinda.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...