[MW:12290] Radiography of joint at intersection

Dear all,
 
Please tell me is it required to take radiography at the intersection of long seam and cir. seams in a pressure vessel fabrication as per section VIII div. 1.

--
With Best Wishes,
 
Imran Khan
 
Cell:+966580790536
   

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS