Re: [MW:12286] Tensile Test for IS2062 Plates / Coil (Transverse or Longitudinal)

Transverse direction if the plate width is more than 600mm

2011/8/19 Ravi Karuskar <rkaruskar@gmail.com>
Dear Experts,

We are going to manufacture IS 2062 structure. In that case we need to
purchase IS 2062 Coils/Plates. Hence, we need to confirm the material
with the help of chemical and mechanical testing.

Regading chemical testing code given different types of data against
different compositon but i have a querry regarding tensile testing
(Transverse or Longitudinal)

Which tensile testing to be carried out for confirming the plates / coil.


--
Ravi Karuskar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...