[MW:12269] Difference between SB625 UNS NO8904 & SA 240 Type 904L

Dear All Experts,
 
I want to know about the Difference between ASME SB625 UNS NO8904 & ASME SA 240 Type 904L,
 
I have checked chemical and physical properties which are same for both, but still Inspector is demanding for SB 625 Plate instead of ASME SA 240 Type 304 plate.
 
Regards,
 
Kapil Bhamburdekar
QA Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.