Ashish Yadav,
 
How much is greater ?
 
How do you setup the cooling rate in Sysweld and how much you assumed the arc efficiency , What type of heat input model?
 
The above factors have dramtaic impact on the resulst.
 
I was simulated the Autogeneous TIG welding with sysweld2006, i have got as much as 16% variation from the mock up values.
 
 
 
On Thu, Jun 30, 2011 at 3:40 PM, ashish yadav <yadavashish018@gmail.com> wrote:
Hello frnds
                I have done a laser welding simulation using
SYSWELD.In mechanical results I am getting the thermal stress values
greater than yield strength of metal(stainless steel).
How can I justify this.
Please help me.

--
Regards
Ashish Yadav

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
Welding  & Metallurgical Engineer,
PPL Shipyard Pte Ltd
Singapore
HP:  +65 94815990
Skype: psgbabu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...