Monday, June 27, 2011

[MW:11494] RE: 11468] Exothermic Electrodes

http://www.contractconnections.co.nz/cadweld.shtml

 

Link above explains the technique and applications.

 

Best Regards,

 

Jim Nystrom

Product Development Engineer
Campbell Applied Physics, Inc.
4790 Golden Foothill Parkway
El Dorado Hills, CA  95762
Direct Tel/Fax: 916.200.3993

jnystrom@campbellap.com

 

P  Please consider the environment before printing this e-mail

 

CONFIDENTIALITY NOTICE: This electronic message and the documents attached hereto (if any) may contain confidential information belonging to the sender which is legally protected. The information is intended solely for the use of the individual (s) named above. If you are not an intended recipient you are hereby notified that any disclosure, copying, distribution or the taking of any action in reliance on or regarding the contents of this electronic message is strictly prohibited. If you have received this electronic message in error please notify us immediately and permanently delete the original and any copies of this message including any attachments.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of limesh M
Sent: Saturday, June 25, 2011 12:54 AM
To: Materials & Welding
Subject: [MW:11468] Exothermic Electrodes

 

Dear All,

Is there any electrodes called Exothermic Electrodes?


Regards,

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...