Mr Muni,

in my opinion if you want to Approve any PQR and WPQ acc. ASME with
3rd part (ASME allows you to approve PQR and WPQ by your own if you
don't have special requirements from your client ) best way to do this
is perform samples with Authorized ASME Inspector as witness. As I
know DNV in Poland don't have Authorized Inspector like TUV NORD,
Lloyd Register or TUV Rheinland.
For example on website of DNV Poland in category welders certification
you don't have ASME code mention.

http://www.dnv.pl/industry/maritime/servicessolutions/certyfikacja_spawaczy/index.asp

On 27 Cze, 21:30, Muni Andy <cmkf...@gmail.com> wrote:
> Mr.Raja,
> Can you tel me why DNV cannot witness test and Approve PQR n WPQ as per
> ASME?
> MuniOn Fri, Jun 24, 2011 at 1:29 PM, graja <agrajew...@gmail.com> wrote:
> > Hi,
>
> > as I know UDT and DNV Poland don't have ASME authorized inspector to
> > approve or coordinate welding acc. ASME, but TUV NORD, TUV Rheinland
> > or Lloyd Register in Poland have ASME authorized inspector so you can
> > ask them about ASME subject.
>
> > I work a little beat with ASME and if you don't have special
> > requirements about 3rd part you can approved PQR and WPQ by yourself.
>
> > sorry for my English, I have hope I help.
>
> > On Jun 23, 4:17 am, <vinit.deshpa...@akersolutions.com> wrote:
> > > Dear Experts,
>
> > > Need you your Help.
>
> > > One of our supplier has informed us that ''We cannot perform welding
> > according to ASME because DNV Poland don't have accreditation for ASME''.
>
> > > As per my knowledge UDT is-Office of Technical Inspection working as an
> > Inspection Body, as the Notified Body and the Recognized Third Party
> > Organization as the Certification Body.
>
> > > Hence its a Inspection body only, my questions are as below,
>
> > > Is my understanding about UDT is correct?
>
> > > Can we do welding as per ASME in Poland?
>
> > > What are the options to be considered If we need to do welding in Poland
> > according to ASME.
>
> > > Your early reply in this regard is appreciated
>
> > > Regards,
> > > Vinit Deshpande
> > > Aker Solutions
> > > Tel: +47-67826358
> > > Mobile: +47-45217814
> > > Email: Vinit.Deshpa...@akersolutions.com
>
> > > -
> > > This e-mail and any attachment are confidential and may be privileged or
> > otherwise protected from disclosure. It is solely intended for the person(s)
> > named above. If you are not the intended recipient, any reading, use,
> > disclosure, copying or distribution of all or parts of this e-mail or
> > associated attachments is strictly prohibited. If you are not an intended
> > recipient, please notify the sender immediately by replying to this message
> > or by telephone and delete this email and any attachments permanently from
> > your system.
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...