Dear Sir

1. Before pressuring the lines, each weld joint shall be
cleaned by wire brush or power brush to free it from rust and any
other foreign matter.So at any way don't allow painting or priming
before hydrotesting.

2. If you are going to UT or MPI (NDT) -- You will not get proper
Intrpretuation result and smooth movement of probe is also not
possible.So don't allow painting.

3. If your NDT method is RT then you can continue painting.(After hydro)


Madhusoodhanan Nair.G
Sr Inspector , Velosi(I)

09967901872

On 6/29/11, santoshcwi@gmail.com <santoshcwi@gmail.com> wrote:
> Dear Mr. Dheerendran,
> please mention which NDE method you need to carry out on the pipeline
>
>
> Regards
>
> Santosh Gaikwad
> Sent on my BlackBerry® from Vodafone
>
> -----Original Message-----
> From: dheerendra chauhan <chauhandheerendra@gmail.com>
> Sender: materials-welding@googlegroups.com
> Date: Wed, 29 Jun 2011 12:08:15
> To: <materials-welding@googlegroups.com>
> Reply-To: materials-welding@googlegroups.com
> Subject: [MW:11513] NDT on Pipe line for Natural gas
>
> Gents,
> we are fabricating a Pipe line for Natural gas . Now the contractor has done
> Primer on Joints also before the NDT testing.
>
> How it is going to affect it & what are the remedy for that.
>
> --
> Thanks & Regards
>
> Dheerendra Singh Chauhan
> Project Manager
> Powergas International
> +234-7055215480
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...