Wednesday, June 29, 2011

[MW:11506] Re: Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE

Dear mohd,

In all case it not a problems.Just inform mfg to submitted written
approval from client.
and attached this approval with your inspection report and submitte
cleint to approve your report.

1.Inform client to add this joint in his drawing and apprvoed same as
it is.
2. this is between you and cleint.(code is slient about this)

regards,
mohd.

"MANUFACTURER IS SAYING THEY HAVE APPROVAL FROM CLIENTS ABOUT ABOVE
MENTIONED ISSUE"

n Jun 28, 5:42 pm, Nandesh Kumar <nandeshku...@rocketmail.com> wrote:
> Hi Mohamad,
>
> Refer Appendix J of API 5L . u will find PSL1 and PSL2 differences.
>
> Nandeesh
> Fahaheel
>
> --- On Mon, 27/6/11, sajidalam mohd. <engineer_makes_wo...@yahoo.co.in> wrote:
>
> From: sajidalam mohd. <engineer_makes_wo...@yahoo.co.in>
> Subject: [MW:11497] Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE
> To: materials-welding@googlegroups.com
> Date: Monday, 27 June, 2011, 11:41 PM
>
> DEAR EXPERTS
>                  WHAT IS DIFFERANCE BETWEEN PSL1 & PSL 2 CARBON STEEL PIPE.
>   
> I AM DOING INSPECTION FOR PSL2 CARBON STEEL PIPES (BY SAW PROSESS AS PER API5L).
>   
> OUR PIPE'S LENGTH ACCEPTANCE CRITERIA IS 12 METER TO 18 METER.
>  
>  
> MANUFACTURER HAS SO MANY SHORT LENGTH PIPES LIKE AS 8 METER, 7 METER & 10 METER.
>  
> HE WANTS TO JOINT TWO SHORT LENGTH PIPES BY SMAW PROCESS.
>  
> I WANT TO ASK THAT IF MANUFACTURER IS JOINING TWO SHORT LENGTH PIPES THAT PIPE WILL BE ACCEPTED AS PER API5L FOR PSL2.
>  
> MANUFACTURER IS SAYING THEY HAVE APPROVAL FROM CLIENTS ABOUT ABOVE MENTIONED ISSUE.ME SHOULD GIVE RELEASE FOR THAT PIPES OR NOT.
>  
> IT IS ALLOW OR NOT/AND WHERE IT IS MENTIONED THAT FOR PSL2 PIPES IF LENGTH ACCEPTANCE CRITERIA IS MENTIONED BY CLIENTS/API5L AFTERTHAT MANUFACTURER WILL JOIN TWO SHORT LENGTH PIPE AND HE WILL PROCESS THAT PIPES AS  PER PSL2  PIPES.
>   
>   
> REGARDS
> MOHAMMAD SAJID ALAM
> INSPECTION ENGINEER
> KUWAIT
>  
>  
>
> --
>
> To post to this group, send email to materials-welding@googlegroups.com
>
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
>
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...