RE: [MW:11503] Difference between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE
Dear Sajid,
Find attached here with difference between PSL 1& PSL 2. Further impact test required for PSL 2 vice versa PSL 1.
Vimal Mistry
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sajidalam mohd.
Sent: Tuesday, June 28, 2011 5:12 AM
To: materials-welding@googlegroups.com
Subject: [MW:11497] Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE
| DEAR EXPERTS WHAT IS DIFFERANCE BETWEEN PSL1 & PSL 2 CARBON STEEL PIPE. I AM DOING INSPECTION FOR PSL2 CARBON STEEL PIPES (BY SAW PROSESS AS PER API5L). OUR PIPE'S LENGTH ACCEPTANCE CRITERIA IS 12 METER TO 18 METER. MANUFACTURER HAS SO MANY SHORT LENGTH PIPES LIKE AS 8 METER, 7 METER & 10 METER. HE WANTS TO JOINT TWO SHORT LENGTH PIPES BY SMAW PROCESS. I WANT TO ASK THAT IF MANUFACTURER IS JOINING TWO SHORT LENGTH PIPES THAT PIPE WILL BE ACCEPTED AS PER API5L FOR PSL2. MANUFACTURER IS SAYING THEY HAVE APPROVAL FROM CLIENTS ABOUT ABOVE MENTIONED ISSUE.ME SHOULD GIVE RELEASE FOR THAT PIPES OR NOT. IT IS ALLOW OR NOT/AND WHERE IT IS MENTIONED THAT FOR PSL2 PIPES IF LENGTH ACCEPTANCE CRITERIA IS MENTIONED BY CLIENTS/API5L AFTERTHAT MANUFACTURER WILL JOIN TWO SHORT LENGTH PIPE AND HE WILL PROCESS THAT PIPES AS PER PSL2 PIPES. REGARDS MOHAMMAD SAJID ALAM INSPECTION ENGINEER KUWAIT |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
- Disclaimer--
This email and any files transmitted with it are confidential and may be privileged or otherwise protected from disclosure and are intended solely for the use of the entity / individual to whom they are addressed. If you have received this email in error or If you are not the intended recipient, please notify the sender immediately by way of telephone or email and delete this message and any files transmitted from your system. Please note that any views presented in the email are solely those of the author and do not necessarily represent those of the organization. While all care has been taken to avoid viruses the recipient is advised to check this email and attachments for presence of viruses. The organization accepts no liability on this account.
Comments