Tuesday, June 28, 2011

[MW:11497] Differance between PSL1 AND PSL2 PIPE/SHORT LENGTH JOINTES PIPE ISSUE/PSL2 CARBON STEEL PIPE

DEAR EXPERTS

                 WHAT IS DIFFERANCE BETWEEN PSL1 & PSL 2 CARBON STEEL PIPE.

 

I AM DOING INSPECTION FOR PSL2 CARBON STEEL PIPES (BY SAW PROSESS AS PER API5L).

 

OUR PIPE'S LENGTH ACCEPTANCE CRITERIA IS 12 METER TO 18 METER.

 

 

MANUFACTURER HAS SO MANY SHORT LENGTH PIPES LIKE AS 8 METER, 7 METER & 10 METER.

 

HE WANTS TO JOINT TWO SHORT LENGTH PIPES BY SMAW PROCESS.

 

I WANT TO ASK THAT IF MANUFACTURER IS JOINING TWO SHORT LENGTH PIPES THAT PIPE WILL BE ACCEPTED AS PER API5L FOR PSL2.

 

MANUFACTURER IS SAYING THEY HAVE APPROVAL FROM CLIENTS ABOUT ABOVE MENTIONED ISSUE.ME SHOULD GIVE RELEASE FOR THAT PIPES OR NOT.

 

IT IS ALLOW OR NOT/AND WHERE IT IS MENTIONED THAT FOR PSL2 PIPES IF LENGTH ACCEPTANCE CRITERIA IS MENTIONED BY CLIENTS/API5L AFTERTHAT MANUFACTURER WILL JOIN TWO SHORT LENGTH PIPE AND HE WILL PROCESS THAT PIPES AS  PER PSL2  PIPES.

 

 

REGARDS

MOHAMMAD SAJID ALAM

INSPECTION ENGINEER

KUWAIT

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...