Re: [MW:11520] vertical down welding qualification

Hi Dias,
 
The reason Vertical Weling is a challenge is combating gravity, For vertical SMAW E7018 is most suitable electrode because of their low iron pwder content, the molten metal produces a puddle that can freeze quickly and is less inclined to drip off the work during liquid state, also note E7018 is low hydrogen electrode.
 
If you want to make an effort to increase deposition rates choose small diameter (1.2mm) gas shielded FCAW electrode E71T-1 or E71T-12, offer good eposition rates when used for Out of Position welding, the slag is designed to support the puddle when welding vertical up or overhead.
 
Please recheck Client spec carefully since some of the client spec i am aware restrict Vertical welding to upward direction only and need approval for Downwards, Also changing Up to down is supplemetary variable in ASME sec ix,
 
I would suggest to go with FCAW widely used with succesful maechanical results.
Should you have further query, please let me know.
 
Regards
Manpreet Singh
 


From: "Hepolito Dias"hepolitodias@gmail.com
Sent: Wed, 29 Jun 2011 17:38:19 +0530
To: materials-welding@googlegroups.com
Subject: [MW:11502] vertical down welding qualification

Hello all
we are on a regular basis doing a job involving a lot of vertical welding of stiffeners 16 mm thk base metal general carbon steel 0.1 to 0.2 C group.
The same is as per client specs being done by E 7018 in normal position.
Iam looking for details on qualificationand approvals in vertical down positionif anyone has the samefor SMAW or even MAG using low hydrogen electrodes like E 7016 [or equivalent in MAG ] to reduce production time on the job drastically.
 

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...