Re: [MW:11469] Dilution

Dear Maulik,

The formula which u have given is correct. But for % of element in weld metal will vary bead by bead. And also for which element shall we calculate? Because element wise laso dilution will change. So in this case what should be taken as reference?

On Fri, Jun 24, 2011 at 9:33 PM, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:
Dear Vicky,
 
Dilution= [% of a element in base metal (by PMI/by TC)-% of a element in weld metal (by PMI/by Chemical testing)-%of a element in filler wire (got it by TC/SEC IIC)] whole divided by % of a element in base metal.
 
Then deduct product from 1 & multiply product to 100.

On Fri, Apr 22, 2011 at 10:23 PM, Vicky Bangar <bangarvicky007@gmail.com> wrote:
Dear sir,
           How to measure dilution in Electroslag Strip Cladding (ESSC)? From macrophotograph it is possible to measure are of diluted base metal and total overlay area. But how to check dilution by chemistry method? How much is percentage dilution expected in ESSC? With higher strip width does dilution changes? What will be effect of base metal thickness on dilution? What are recommended base metal thicknesses for using 60 and 90 wide strips? 

--
Vivek Bangar
B.Tech. Metallurgy and Material Science.
Larsen & Toubro Limited,
Powai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Vivek Bangar
B.Tech. Metallurgy and Material Science.
Larsen & Toubro Limited,
Powai

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...