Monday, June 27, 2011

[MW:11486] Re: Temper embrittlement

Dear maulik,

Temper embritllement can be prevented by keeping sulfer an phosferous
at low level and also addition of Mo(<0.15% min) will prevent temper
embritllent.

As far as my interpretaion SecIX all P5B materials have a more than
0.5%Mo. so that not required.

It really intersting subject..if get more info please share with us.

regards,
mohd.


On Jun 26, 11:28 am, "Maulik H. Thakkar" <mlkthakk...@gmail.com>
wrote:
> Dear all,
>
> Why temper embrittlement test is not required for P5B materials as per
> API 934?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...