Re: [MW:11456] MPI forgotten

I think madhusoodhanan is right, UT if far more better inspection technique compared to MPI, but then again there might be some discontinuity that could be detected.
 


 
On Fri, Jun 24, 2011 at 2:21 AM, madhusoodhanan nair <nairdan2@gmail.com> wrote:
Dear Vagal


          You can clear the joint with ultrasonic inspection without
cutting and rewelding.



On 6/24/11, Shashank Vagal <nach_sam@yahoo.com> wrote:
> Dear members,
> By some oversight, MPI of one pipeline welds was not done on cut bevels. The
> PL section is now ready for hydrotest. Construction Code is API 1104 1999
> Ed.
> RT is acceptable. But this lapse is punchlisted. How do you resolve the
> issue?
> Cutting and rewelding is not permitted.
> Best regards,
> Shashank Vagal
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...