Monday, May 30, 2011

RE: [MW:11210] Welding consumable for CD3Mn

You can use Duplex 2209 AC-DC it is specially formulated for welding Type 2205 combining with high strength with improved pitting & SCC resistance.

Smooth running arc gives you uniform bead.

 

 

Cheers!!!!

J

 

Regards,
Prakash Verma
Aker Drilling Risers
Aker Solutions
MOBILE - 0047-40466591
DESK- 0047-22945932
Email: Prakash.Verma@akersolutions.com


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of fredric prabu
Sent: 30. mai 2011 07:21
To: materials-welding@googlegroups.com
Subject: [MW:11202] Welding consumable for CD3Mn

 

Dear experts

 

Can some body suggest suitable welding consumable for welding casting grade CD3Mn , UNS J92205 in SMAW process.

 

Thanks

 

Regards

Fredric prabu


This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...