I have confirmed with ASME that this an error – it will be corrected in the 2011 edition of Sc IX.
Use P-No. 15E
John
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vanchinath S.A.
Sent: Saturday, May 21, 2011 10:02 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11111] RE: 11080] SA-213 Gr.T91
P no. 15E is correct
vanchi
On Wed, May 18, 2011 at 9:51 PM, John Henning <jhenning@deltak.com> wrote:
Appears to be an error. All UNS K90901 (“91” alloy) were to be changed to P-No. 15E with publishing of 2009 Edition.
Use P-No. 15E
John
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of srinivasu
Sent: Wednesday, May 18, 2011 4:40 AM
To: materials-welding@googlegroups.com
Subject: [MW:11080] SA-213 Gr.T91
Dear Experts
What's the P.No. of Material Specification of SA-213 Gr.T91?
I refer Sec.IX 2010 Edition as per QW-422 - it's P.No.5B Gr.No.2
as per Appendices-D - it's mentioned P.No.15E Gr.No.1
Which one is the correct?
With Regards
Srinivasu V
Welding Engineer
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments