[MW:11170] Re: Pickling Passivation of Hastalloy

I have already downloaded info. from suggested site but to have more
authentic reference
I need to know ASTM standard for this.

Please help me out.

Best regards,

Prasad

On May 27, 11:28 am, jignesh.r...@Linde-LE.com wrote:
> Dear Mr. Prasad,
>
> Referwww.haynesintl.com.
>
>  It suggest some recommendations for pickling and passivation for
> hastalloy.
>
> After PWHT, the oxide film is more adherent than normal 18/8 grade
> stainless steel.  Molten caustic  bath followed by acid pickling found to
> be most suitable method.
>
> With Best Regards,
>
> Jignesh R Rana
> Manager - Materials Technology, QA/QC & Standards
>
> Linde AG
> Linde Engineering Division
> Dr.-Carl-von-Linde-Str. 6 - 14
> 82049 Pullach / Germany
> phone:    +49 89 7445 - 2360
> fax:           +49 89 7445 - 4952
> e-mail:    jignesh.r...@linde-le.com
> web:        http://www.linde.com
>
> This e-mail is confidential. If you are not the intended recipient, please
> notify us immediately. You should not disclose its contents to any other
> person nor use it for any purposes.
>
> Prasad <prs...@gmail.com>
> Sent by: materials-welding@googlegroups.com
> 27.05.11 05:50
> Please respond to
> materials-welding@googlegroups.com
>
> To
> "Materials & Welding" <materials-welding@googlegroups.com>
> cc
>
> Subject
> [MW:11160] Pickling Passivation of Hastalloy
>
> Dear experts,
>
> We are fabricating a pressure vessel with Hastalloy claded plates.
> Vessel is to undergo PWHT. I would like to know which is the ASTM
> standard covers
> pickling of Hastalloy material, like A380 is for SS materials.
> Code of construction is ASME Sec. VIII Div. 1 2007.
>
> THanking you in advance.
>
> Prasad
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

Bestblogger said...

I appreciate you sharing this blog. Excellent blog for me.

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...