Friday, May 27, 2011

Re: [MW:11164] Pickling Passivation of Hastalloy

Dear Mr. Prasad,

Refer www.haynesintl.com .

 It suggest some recommendations for pickling and passivation for hastalloy.

After PWHT, the oxide film is more adherent than normal 18/8 grade stainless steel.  Molten caustic  bath followed by acid pickling found to be most suitable method.

With Best Regards,

Jignesh R Rana
Manager - Materials Technology, QA/QC & Standards

Linde AG
Linde Engineering Division
Dr.-Carl-von-Linde-Str. 6 - 14
82049 Pullach / Germany
phone:    +49 89 7445 - 2360
fax:           +49 89 7445 - 4952    
e-mail:    jignesh.rana@linde-le.com
web:        
http://www.linde.com


This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.





Prasad <prsgne@gmail.com>
Sent by: materials-welding@googlegroups.com

27.05.11 05:50

Please respond to
materials-welding@googlegroups.com

To
"Materials & Welding" <materials-welding@googlegroups.com>
cc
Subject
[MW:11160] Pickling Passivation of Hastalloy





Dear experts,

We are fabricating a pressure vessel with Hastalloy claded plates.
Vessel is to undergo PWHT. I would like to know which is the ASTM
standard covers
pickling of Hastalloy material, like A380 is for SS materials.
Code of construction is ASME Sec. VIII Div. 1 2007.

THanking you in advance.

Prasad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...