Dear All,

One of my client told me to incorporate in water fillup test procedure that inhibitors to be added in the water using for water fillup test. My doubt is when we are using potable water for testing is it required to add inhibitors and can u give me some information about the disposal of water (disposal procedure) after testing.

Thanks in advance.
Manoj 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...